SPECIFICATION:
Appearance | White powder |
P % | 13.5 min |
N % | 35 min |
Decomposition temperature ℃ | 300 min |
Solubility(25℃,g/100ml water) | 0.1 max |
Particle size(D50) | 15 μm |
APPLICATION:
1. MPP can be used as catalyst and foaming agent in fireproof coating, and its performance is slightly better than that of common ammonium polyphosphate.
2. It can be applied in vinyl acetate copolymer such as sharing with cyclic urea-formaldehyde (coking agent) in polyolefin demonstrating highly effective expansion flame retardant effect.
3. It is an effective flame retardant used in combination with pentaerythritol phosphate in thermoplastic polyester.
4. It is suitable for making polystyrene flame retardant, instead of polybrominated diphenyl ether.
5. It is suitable for making rubber (butadiene, nitrile, polypropylene elastic) nylon 6/6, epoxy resin, hard polyurethane foam flame retardant.
PACKING:
25 kg net bags